Not your region? Change it here:
Sodium Silicate Binder consisting of 83% rapid water soluble sodium water glass and 17% water, acid and lye insoluble binder additives. Ankerglas-SN33 and Ankerglas-SN27 have a different Mol ratio SiO2:Na2O. Ankerglas-SN33 has a lower and SN27 a higher dissolving velocity. Ankerglas-SN33 has a better shelf life.
Sales Manager
Ankerglas-SN33 and Ankerglas-SN27 have been specially developed as a silicate based binder for ceramics. The main application is in refractory gunning and centrifugal masses.
Calcined Bauxite is produced by the sintering/calcining of low-iron, low-alkali containing raw bauxites at temperatures of 1600 – 1800°C. In this calcination process the hi...
Caustic Calcined Magnesia (CCM) is a mineral raw material produced by calcining magnesium carbonate at high temperatures. It is characterized by high purity and excellent c...
During sintering (firing) at temperatures of 1750 – 2000 C° in shaft or rotary kilns naturally occurring magnesium carbonate is converted into sintered magnesia, directly (...